    This hot-rolled structural steel offers excellent weldability for ease of processing.

    We exercise stringent control over the chemical composition and mechanical properties of our ship plate – ensuring products of consistent and reliable quality for demanding marine applications.

    Hot rolled steel for enhanced end performance

    Ympress® Laser offers fast, efficient laser-cutting with superior performance.

    Specially prepared to enable fast cutting with a clean cut edge, it is ideal for automated processing and guarantees production efficiency and consistency.

    Contact us

    Tata Steel

    PO Box 10.000

    1970 CA IJmuiden

    Netherlands

    Helpdesk

    T +31 (0)251 494191

    Overview

     

    Relationship with standards

    Ship plate is normally supplied according to Lloyds EMEA (Europe, Middle East and Africa) grade A and grade B.

    Grade A is also available according to Germanischer Lloyds.

     

     

    back to top

    Properties

     

    Mechanical properties

    Ship plate has the following mechanical properties, measured transverse to the rolling direction:

    Lloyds EMEA Grade

    Min. yield strength 1
    ReH

    Tensile strength
    Rm

    Min. elongation after fracture A

    Impact test

     

     

    N/mm²

    N/mm²

    %

     

     

     

     

     

    L0 = 5.65√S0

    Temp. °C

    min. energy J

    Grade A

    235

    400 - 520

    22

    -

    -

    Grade B

    235

    400 - 520

    22

    0

    27 (l)/ 20 (t) 2

    1. Upper yield strength applies.
    2. l is measured longitudinal to the rolling direction; t is measured transverse to the rolling direction.

     

    Chemical composition

    Tata Steel will satisfy the following cast analysis with maximum values in weight percentages:

    Lloyds EMEA

    C

    Mn

    P

    S

    Si

    Alsol

     

    Max.

    Min.

    Max.

    Max.

    Max.

    Min.

    Grade A

    0.21

    -

    0.035

    0.035

    0.50

    0.02

    Grade B

    0.21

    0.80

    0.035

    0.035

    0.35

    0.02

     

     

    back to top

    Dimensions

     

    Dimensional Capability

    Dimensions in mm.

    Thickness

    Max. width

    From - up to

    Grade A

    Grade B

    1.49 - 1.60

    1170

    1170

    1.60 - 1.70

    1280

    1280

    1.70 - 1.80

    1370

    1370

    1.80 - 1.90

    1440

    1440

    1.90 - 2.00

    1520

    1520

    2.00 - 2.20

    1590

    1590

    2.20 - 2.40

    1730

    1730

    2.40 - 2.60

    1800

    1800

    2.60 - 2.80

    1880

    1880

    2.80 - 3.12

    1960

    1960

    3.12 - 12.70

    2070

    2070

    12.70 - 20.00

    2070

    2070

    Minimum width is 900mm.
    Widths smaller than 900mm are available on request - please contact us.

     

    Tolerances

    Tolerances for wide strip and slit wide strip comply with standard EN 10051: 2010 (click here).

    Tighter tolerances are available, please contact us.

     

     

    back to top

    Overview

    Overview

     

    Relationship with standards

    Ship plate is normally supplied according to Lloyds EMEA (Europe, Middle East and Africa) grade A and grade B.

    Grade A is also available according to Germanischer Lloyds.

     

     

    back to top

    Properties

    Properties

     

    Mechanical properties

    Ship plate has the following mechanical properties, measured transverse to the rolling direction:

    Lloyds EMEA Grade

    Min. yield strength 1
    ReH

    Tensile strength
    Rm

    Min. elongation after fracture A

    Impact test

     

     

    N/mm²

    N/mm²

    %

     

     

     

     

     

    L0 = 5.65√S0

    Temp. °C

    min. energy J

    Grade A

    235

    400 - 520

    22

    -

    -

    Grade B

    235

    400 - 520

    22

    0

    27 (l)/ 20 (t) 2

    1. Upper yield strength applies.
    2. l is measured longitudinal to the rolling direction; t is measured transverse to the rolling direction.

     

    Chemical composition

    Tata Steel will satisfy the following cast analysis with maximum values in weight percentages:

    Lloyds EMEA

    C

    Mn

    P

    S

    Si

    Alsol

     

    Max.

    Min.

    Max.

    Max.

    Max.

    Min.

    Grade A

    0.21

    -

    0.035

    0.035

    0.50

    0.02

    Grade B

    0.21

    0.80

    0.035

    0.035

    0.35

    0.02

     

     

    back to top

    Dimensions

    Dimensions

     

    Dimensional Capability

    Dimensions in mm.

    Thickness

    Max. width

    From - up to

    Grade A

    Grade B

    1.49 - 1.60

    1170

    1170

    1.60 - 1.70

    1280

    1280

    1.70 - 1.80

    1370

    1370

    1.80 - 1.90

    1440

    1440

    1.90 - 2.00

    1520

    1520

    2.00 - 2.20

    1590

    1590

    2.20 - 2.40

    1730

    1730

    2.40 - 2.60

    1800

    1800

    2.60 - 2.80

    1880

    1880

    2.80 - 3.12

    1960

    1960

    3.12 - 12.70

    2070

    2070

    12.70 - 20.00

    2070

    2070

    Minimum width is 900mm.
    Widths smaller than 900mm are available on request - please contact us.

     

    Tolerances

    Tolerances for wide strip and slit wide strip comply with standard EN 10051: 2010 (click here).

    Tighter tolerances are available, please contact us.

     

     