Properties

Properties


Mechanical properties

Steel for enamelling has the following mechanical properties (skin-passed) - these are measured transverse to the rolling direction:

Tata Steel Grade Ymvit 04 plus
EN 10209: 2013 Grade DC04EK
Max. yield strength Re 1,2,3 N/mm² 210
Tensile strength Rm N/mm² 270 - 350
Elongation 3 % 38
r-value r90 -
ravg -
FLD Yes/No -
1. The values of the yield strength are those of the 0.2% yield strength for products that do not present a definite yield point, and the lower yield strength ReL for the other products.
2. For a thickness of 0.5 mm < t < 0.7 mm the maximum value of the yield strength is increased by 20 N/mm² and the minimum elongation after fracture is decreased by 2%.
3. For a thickness of t ≤ 0.5 mm the maximum value of the yield strength is increased by 40 N/mm² and the minimum elongation after fracture is decreased by 4%.
   Elongation after fracture A uses test piece length L0 = 80 mm.
4. The r value applies to a thickness of t ≥ 0.5 mm.
   For a thickness of t > 2 mm, the r value is decreased by 0.2.
5. For a thickness of t ≥ 1.5 mm the maximum value of the yield strength is 225 N/mm².
 

Chemical composition

Tata Steel complies with the following cast analysis:

Tata Steel Ymvit Grade Ymvit 04 plus
EN 10209: 2013 Grade DC04EK
C Max. 0.08
Mn Max. 0.40
P Max. 0.030
S Max. 0.050
Ti Max. -
The elements P and Cu are kept within certain limits to ensure that the reactivity of the steel surface is as constant as possible. Under normal conditions this leads to a reproducible enamelling result.