EN 10149-2:2013 |
ReH / Rp |
Rm |
A80 |
Adp5 |
---|---|---|---|---|---|
Grade | Hot-rolled | N/mm² | N/mm² |
% |
% |
|
|
|
|
t < 3.0 |
t ≥ 3.0 |
Ymagine H320-UC |
S315MC |
≥ 315 |
390 - 510 |
≥ 20 |
- |
Ymagine H360-UC |
S355MC |
≥ 355 |
430 - 550 |
≥ 19 |
≥ 23 |
Ymagine H420-UC |
S420MC |
≥ 420 |
480 - 620 |
≥ 16 |
≥ 19 |
Ymagine H500-UC |
S500MC |
≥ 500 |
550 - 700 |
≥ 12 |
≥ 14 |
t - material thickness in mm.
Tata Steel |
EN 10268:2006: longitudinal |
Rp |
Rm |
A80 |
---|---|---|---|---|
Grade |
Cold-rolled |
N/mm² |
N/mm² |
% |
Ymagine H240-UC |
HC260LA |
240 - 310 |
340 - 420 |
≥ 27 |
Ymagine H320-UC |
HC340LA |
320 - 410 |
400 - 500 |
≥ 22 |
Ymagine H360-UC |
HC380LA |
360 - 460 |
430 - 550 |
≥ 20 |
Ymagine H420-UC |
HC420LA |
400 - 500 |
460 - 580 |
≥ 18 |