Overview
Applications
Domestic appliances
Furniture
Tubing
Racking and shelving
Pressure vessels
Home
Products
Engineering
Cold-rolled
Structural steel
Cold-rolled - Structural steel
Our structural steel is suitable for a wide range of applications.
It has a guaranteed minimum strength and offers good weldability for ease of processing.
Our advanced and ultra high-strength cold-rolled steels DP600, DP800, DP1000 and HQ1500 are lightweight and enable design freedom for complex parts.
Their high yield and ductility ensure shape accuracy and tolerancing, which enable thickness reduction and maintained in-service performance for difficult-to-form parts.
Cold-rolled structural steel has the following mechanical properties (skin-passed) - these are measured transverse to the rolling direction:
Grade |
Yield strength 1 Rp |
Tensile strength 1 Rm |
Min. elongation after fracture A |
---|---|---|---|
|
N/mm2 |
N/mm2 |
% |
CA200 |
200 - 260 |
320 - 380 |
30 |
CA240 |
240 - 300 |
340 - 400 |
28 |
1. Lower yield point or 0.2% proof stress applies.
There are no direct EN standard equivalents.
Cast analysis with maximum values in weight percentages:
|
C |
Mn |
P |
S |
Sol. Al |
---|---|---|---|---|---|
Grade |
Max. |
Max. |
Max. |
Max. |
Min. - Max. |
CA200 |
0.085 |
0.55 |
0.03 |
0.03 |
0.015 - 0.080 |
CA240 |
0.085 |
0.55 |
0.03 |
0.03 |
0.020 - 0.080 |
Continuously-annealed (CA) products.
Dimensions in mm.
Thickness | Max. width | |
---|---|---|
From - up to | CA200 | CA240 |
0.37 - 0.38 | 1390 | - |
0.38 - 0.40 | 1390 | 1390 |
0.45 - 0.50 | 1470 | 1390 |
0.50 - 0.60 | 1550 | 1515 |
0.60 - 0.65 | 1600 | 1600 |
0.65 - 0.70 | 1710 | 1600 |
0.70 - 0.75 | 1710 | 1710 |
0.75 - 0.90 | 1710 | 1710 |
0.90 - 0.95 | 1820 | 1820 |
0.95 - 1.60 | 1820 | 1820 |
1.60 - 1.70 | 1750 | 1750 |
1.70 - 1.80 | 1650 | 1620 |
1.80 - 1.90 | 1525 | 1500 |
1.90 - 2.00 | 1500 | 1500 |
Minimum width is 900mm for thicknesses below 0.5mm.
Minimum width is 825mm for all other thicknesses.
Tolerances comply with standard EN 10131: 2006 (click here).
Tighter tolerances are available, please contact us for details.
Jump to
Overview
Properties
Cold-rolled structural steel has the following mechanical properties (skin-passed) - these are measured transverse to the rolling direction:
Grade |
Yield strength 1 Rp |
Tensile strength 1 Rm |
Min. elongation after fracture A |
---|---|---|---|
|
N/mm2 |
N/mm2 |
% |
CA200 |
200 - 260 |
320 - 380 |
30 |
CA240 |
240 - 300 |
340 - 400 |
28 |
1. Lower yield point or 0.2% proof stress applies.
There are no direct EN standard equivalents.
Cast analysis with maximum values in weight percentages:
|
C |
Mn |
P |
S |
Sol. Al |
---|---|---|---|---|---|
Grade |
Max. |
Max. |
Max. |
Max. |
Min. - Max. |
CA200 |
0.085 |
0.55 |
0.03 |
0.03 |
0.015 - 0.080 |
CA240 |
0.085 |
0.55 |
0.03 |
0.03 |
0.020 - 0.080 |
Dimensions
Continuously-annealed (CA) products.
Dimensions in mm.
Thickness | Max. width | |
---|---|---|
From - up to | CA200 | CA240 |
0.37 - 0.38 | 1390 | - |
0.38 - 0.40 | 1390 | 1390 |
0.45 - 0.50 | 1470 | 1390 |
0.50 - 0.60 | 1550 | 1515 |
0.60 - 0.65 | 1600 | 1600 |
0.65 - 0.70 | 1710 | 1600 |
0.70 - 0.75 | 1710 | 1710 |
0.75 - 0.90 | 1710 | 1710 |
0.90 - 0.95 | 1820 | 1820 |
0.95 - 1.60 | 1820 | 1820 |
1.60 - 1.70 | 1750 | 1750 |
1.70 - 1.80 | 1650 | 1620 |
1.80 - 1.90 | 1525 | 1500 |
1.90 - 2.00 | 1500 | 1500 |
Minimum width is 900mm for thicknesses below 0.5mm.
Minimum width is 825mm for all other thicknesses.
Tolerances comply with standard EN 10131: 2006 (click here).