Hot-rolled

Steel for ship plate

This hot-rolled structural steel offers excellent weldability for ease of processing.

We exercise stringent control over the chemical composition and mechanical properties of our ship plate – ensuring products of consistent and reliable quality for demanding marine applications. 

This is proven by an approval of manufacturer from DNV-GL and Lloyds EMEA.

 

Abrasion resistant wear steel
Product specification
Ship plate is currently available in the following grades

EN-Engineering-Product-Hot-Rolled-Ship plate-Grade A TSN

Grade A
Specification details for Grade A

EN-EngineeringAutomotive-Product-Hot-rolled-All Grades Surface aspects Supply Conditions TSE

Supply Conditions

Supply - product conditions

Hot-rolled steel can be supplied with these product conditions and finishes and with this surface treatment:

Side/surface condition non-pickled pickled pickled and oiled
Mill edges Yes Yes Yes
Trimmed edges - Yes Yes
Trimmed edges available in thicknesses up to 8.0 mm.
Please contact us regarding other specifications we may have that meet your needs.
 

Surface aspects

Description Availability
Surface finish Coils are available in non-pickled and pickled finish for most grades. 
For grade specific availability, please refer to the dimensional tables.
Oiling Pickled finish is available with rolling
or preservative oil applied. 
Oil weight normally 0.5-2.5 g/m2
Alternative oiling ranges are available.
Please contact us for details.
 

Certification

Test certificates 2.2/3.1 are available according to EN 10204.         

EN-Engineering-Product-Hot-Rolled-Ship plate-Grade A-Properties

Properties

Mechanical Properties

Ship plate has the following mechanical properties, measured transverse to the rolling direction:

Lloyds EMEA   Grade A
Min. yield strength ReH 1 N/mm² 235
Tensile strength R N/mm² 400 - 520
Min. elongation after fracture A % 22
Impact test 2 Temp. °C -
Min. energy J -
1. Upper yield strength or 0.2% proof stress applies.
Elongation after fracture A uses test piece length L0 = 5.65√S0.
2. Impact strengths apply to thicknesses > 6 mm and are for standard test pieces only. Please contact us for details.
t – material thickness in mm.

Chemical composition

Tata Steel will satisfy the following cast analysis:

Lloyds EMEA   Grade A
C Max. 0.21
Mn Min. -
P Max. 0.035
S Max. 0.035
Si Max. 0.50
Altot Min. 0.020
All values are in weight%.

EN-Engineering-Product-Hot-Rolled-Ship plate-Grade A-Dimensions

Dimensions

Dimensional capability - non-pickled

Dimensions in mm.

Thickness Max. width
From - up to Grade A
1.49 - 1.60 1170
1.60 - 1.70 1280
1.70 - 1.80 1370
1.80 - 1.90 1440
1.90 - 2.00 1520
2.00 - 2.20 1590
2.20 - 2.40 1730
2.40 - 2.60 1800
2.60 - 2.80 1880
2.80 - 3.12 1960