EN-Engineering-Product-Metallic coated-HSS-All Grades Overview
Relationship with standards
European standard |
|
---|---|
EN 10346:2015 |
|
Phosphorus alloyed interstitial-free |
For phosphorus alloyed interstitial-free grades, bake-hardening grades and phosphorus alloyed grades, please visit the Automotive HSS page. |
HX220YD+Z/+ZF/+ZM |
|
HX260YD+Z/+ZF/+ZM |
|
Bake-hardening |
|
HX180BD+Z/+ZF/+ZM |
|
HX220BD+Z/+ZF/+ZM |
|
HX260BD+Z/+ZF/+ZM |
|
HX300BD+Z/+ZF/+ZM |
|
Phosphorus alloyed |
|
HX220PD+Z 1 |
|
HX260PD+Z 1 |
|
HX300PD+Z 1 |
|
Micro-alloyed |
|
HX220LAD+Z/+ZF/+ZM 1 |
|
HX260LAD+Z/+ZF/+ZM |
|
HX300LAD+Z/+ZF/+ZM |
|
HX340LAD+Z/+ZF/+ZM |
|
HX380LAD+Z/+ZF/+ZM |
|
HX420LAD+Z/+ZM |
|
HX460LAD+Z/+ZM |
|
HX500LAD+Z/+ZM |
1. Not in EN 10346:2015. Tata Steel’s own specification.
EN-Engineering-Product-Metallic coated-All Grades Coatings Surface aspects
Coatings
Three types of metallic coating are available:
Pure zinc
Galvanised steel (+Z) is coated with an almost pure zinc coating (>99% zinc).
Zinc-iron alloy
Galvannealed steel (+ZF) is coated with a zinc coating containing approximately 8-12% iron.
For further information on our galvannealed products please visit our Automotive catalogue.
MagiZinc
MagiZinc steel (+ZM) is coated with a zinc coating containing additional magnesium and aluminium.
Coating weight
Coating | Minimum | Maximum |
---|---|---|
Pure zinc (Z) | 90 (6 µm/side) | 600 (42 µm/side) |
Zinc-iron (ZF) | 90 (6 µm/side) | 140 (10 µm/side) |
MagiZinc (ZM)1 | 70 (5 µm/side) | 310 (22 µm/side) |
Coating weight measured in g/m2 double-sided (µm, per side).
Coils with coatings > 450 g/m2 will be supplied in oscillated coiled condition.
Coils coated with 600 g/m2 are only available in width range 980 to 1300 mm.
1 For MagiZinc (ZM) coating weights below 100 g/m2 please visit our Automotive catalogue.
Surface quality
Surface quality complies with standard: EN 10346:2015. Galvanised steels are available in surface quality A, B or C.
For the highest surface quality requirements we also offer Serica FLO®. For more details please visit our Automotive catalogue.
Surface quality A: as coated surface
Imperfections such as pimples, marks, scratches, pits, variations in surface appearance, dark spots, stripe marks and light passivation stains are permissible.
Stretch levelling breaks or run-off marks may appear. Coil breaks and stretcher strains may also appear.
Surface quality B: improved surface
With this surface quality, small imperfections such as stretch levelling breaks, skin pass marks, slight scratches, indentations, surface structure, zinc run-off marks and light passivation stains are permissible.
Surface quality C: best quality surface
For more information on surface quality C please visit our Automotive catalogue.
Surface finish
Pure zinc
MA: minimised spangle, as coated surface (Z).
MB: minimised spangle, improved surface (Z).
MC: minimised spangle, best quality surface (Z).
Zinc-iron alloy
A: as coated surface (ZF).
B: improved surface (ZF).
C: best quality surface (ZF).
MagiZinc®
A : as coated surface (ZM).
B : improved surface (ZM).
C: best quality surface (ZM).
Surface roughness
Metallic coated steel (with the exception of galvanised steel with standard surface (MA)) can be supplied in various grades of roughness – please contact us for more details. If no roughness is specified, roughness will be as shown in the table below.
Roughness Ra (µm) |
|
---|---|
cut off 0.8mm |
cut off 2.5mm |
0.6 - 1.9 |
0.7 - 2.2 |
Surface treatments
The surface treatments available are O, C and CO.
Oiling (O)
The material surface can be oiled with preservative oil. Other types of oil - for increasing strength or reducing weight – are available to help achieve your optimum performance parameters. Please contact us for details.
Tata Steel offers the following range of oiling levels:
Coating type |
Capability |
---|---|
Pure zinc (Z) |
0.25 - 1.5 g/m2 |
Zinc-iron (ZF) |
0.5 - 1.5 g/m2 |
MagiZinc® (ZM) |
0.25 - 1.5 g/m2 |
Other oiling levels are available on request.
Chromium-free passivation (C)
This surface treatment temporarily protects the zinc-coated material against white rust during transportation and storage (not applicable to all qualities and dimensions – please contact us for details).
Chromium-free passivation and oiled (CO)
Please request this combination of surface treatments if you require extra protection against white rust formation (not applicable to all qualities and dimensions – please contact us for details).
Untreated (U)
Please contact us regarding the availability of untreated coils.
EN-Engineering-Product-Metallic Coated-HSS-HX220LAD-Properties
Properties
Mechanical properties
Metallic coated high-strength steel grades have the following mechanical properties (skin-passed) - these are measured transverse to the rolling direction:
Micro-alloyed steels
Not in EN 10346:2015 | Grade | HX220LAD+Z/+ZF/+ZM |
---|---|---|
Yield strength ReL | N/mm2 | 220 - 300 |
Min. BH2 | N/mm2 | - |
Tensile strength Rm | N/mm2 | 320 - 400 |
Elongation | % | 29 |
Min. r-value | - | |
Min. n-value | - |
Not in EN 10346:2015. Tata Steel’s own specification.
Lower yield strength or 0.2% proof stress applies.
BH2 refers to the increase of 0.2% proof stress after heating (bake hardening). Not applicable for hot rolled substrate.
For galvannealed grades (ZF) the minimum elongation before fracture is lowered by 2%.
For galvannealed grades (ZF) the minimum r90-value is lowered by 0.2.
Chemical composition
Tata Steel supplies the following cast analysis with maximum values unless otherwise shown:
Micro-alloyed steels
Not in EN 10346:2015 | Grade | HX220LAD+Z/+ZF/+ZM |
---|---|---|
C | Max. | 0.10 |
Mn | Max. | 0.60 |
Si | Max. | 0.50 |
P | Max. | 0.03 |
S | Max. | 0.025 |
Altot | Min. | 0.015 |
Ti | Max. | - |
Nb | Max. | - |
Not in EN 10346:2015. Tata Steel’s own specification.
All values are in weight%.
EN-Engineering-Product-Metallic Coated-HSS-HX220LAD-Dimensions
Dimensional capability
Galvanised (+Z) products
Dimensions in mm.
Thickness | Max. width |
---|---|
From - up to | HX220LAD |
0.40 - 0.55 | 1520 |
0.55 - 0.60 | 1580 |
0.60 - 0.65 | 1720 |
0.65 - 0.70 | 1780 |
0.70 - 0.75 | 1800 |
0.75 - 0.90 | 1830 |
0.90 - 1.00 | 1870 |
1.00 - 1.10 | 1930 |
1.10 - 1.20 | 1970 |
1.20 - 1.80 | 2010 |
1.80 - 2.00 | 1920 |
2.00 - 2.20 | 1550 |
2.20 - 3.50 | 1540 |
3.50 - 3.60 | 1450 |
3.60 - 3.70 | 1430 |
3.70 - 3.85 | 1400 |
3.85 - 4.00 | 1350 |
For widths below 900 mm, please contact us.
For thicknesses over 2.50 mm, the minimum width is 1000 mm.
Galvannealed (+ZF) products
For the dimensions of galvannealed (GA) high-strength grades, please contact us.
MagiZinc® (+ZM) products
Dimensions in mm.
Thickness | Max. width |
---|---|
From - up to | HX220LAD |
0.40 - 0.55 | 1520 |
0.55 - 2.00 | 1550 |
For widths below 900 mm, please contact us.
For thicknesses between 2.00 and 2.50 mm, please contact us.
Tolerances
Tolerances comply with standard EN 10143: 2006.
Tighter tolerances are available - please contact us for details.
EN-EngineeringAutomotive-Product-Metallic Coated-All Grades Shape and Dimensional Tolerances
Tolerances on thickness
The tolerances comply with standard EN 10143: 2006.
Tighter tolerances are available on request.
Thickness tolerance availability is shown below:
Thickness tolerance |
Availability |
---|---|
Full thickness tolerance |
Available |
Special thickness tolerance |
Available |
50% of full thickness tolerance |
Refer before ordering |
The following tolerances apply to the grades with a minimum value for the yield strength lower than 260N/mm².
Nominal |
Normal tolerances for a nominal width of 1 2 |
Special tolerances (S) for a |
|||||
---|---|---|---|---|---|---|---|
|
≤ 1200 |
> 1200 |
> 1500 |
≤ 1200 |
> 1200 |
> 1500 |
|
|
≤ 1500 |
|
|
≤ 1500 |
|
||
> 0.40 |
≤ 0.60 |
± 0.04 |
± 0.05 |
± 0.06 |
± 0.035 |
± 0.040 |
± 0.045 |
> 0.60 |
≤ 0.80 |
± 0.05 |
± 0.06 |
± 0.07 |
± 0.040 |
± 0.045 |
± 0.050 |
> 0.80 |
≤ 1.00 |
± 0.06 |
± 0.07 |
± 0.08 |
± 0.045 |
± 0.050 |
± 0.060 |
> 1.00 |
≤ 1.20 |
± 0.07 |
± 0.08 |
± 0.09 |
± 0.050 |
± 0.060 |
± 0.070 |
> 1.20 |
≤ 1.60 |
± 0.10 |
± 0.11 |
± 0.12 |
± 0.060 |
± 0.070 |
± 0.080 |
> 1.60 |
≤ 2.00 |
± 0.12 |
± 0.13 |
± 0.14 |
± 0.070 |
± 0.080 |
± 0.090 |
> 2.00 |
≤ 2.50 |
± 0.14 |
± 0.15 |
± 0.16 |
± 0.090 |
± 0.100 |
± 0.110 |
> 2.50 |
≤ 3.00 |
± 0.17 |
± 0.17 |
± 0.18 |
± 0.110 |
± 0.120 |
± 0.130 |
> 3.00 |
≤ 5.00 |
± 0.20 |
± 0.20 |
± 0.21 |
± 0.15 |
± 0.16 |
± 0.17 |
> 5.00 |
≤ 6.50 |
± 0.22 |
± 0.22 |
± 0.23 |
± 0.17 |
± 0.18 |
± 0.19 |
1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm.
The following tolerances apply to the steel grades with a minimum value for the yield strength 260N/mm² ≤ Rp0.2 < 360N/mm² and for grades DX51D and S550GD.
Nominal |
Normal tolerances for a nominal width of 1 2 |
Special tolerances (S) for a |
|||||
---|---|---|---|---|---|---|---|
|
≤ 1200 |
> 1200 |
> 1500 |
≤ 1200 |
> 1200 |
> 1500 |
|
|
≤ 1500 |
|
|
≤ 1500 |
|
||
≥ 0.35 |
≤ 0.40 |
± 0.05 |
± 0.06 |
- |
± 0.035 |
± 0.040 |
- |
> 0.40 |
≤ 0.60 |
± 0.05 |
± 0.06 |
± 0.07 |
± 0.040 |
± 0.045 |
± 0.050 |
> 0.60 |
≤ 0.80 |
± 0.06 |
± 0.07 |
± 0.08 |
± 0.045 |
± 0.050 |
± 0.060 |
> 0.80 |
≤ 1.00 |
± 0.07 |
± 0.08 |
± 0.09 |
± 0.050 |
± 0.060 |
± 0.070 |
> 1.00 |
≤ 1.20 |
± 0.08 |
± 0.09 |
± 0.11 |
± 0.060 |
± 0.070 |
± 0.080 |
> 1.20 |
≤ 1.60 |
± 0.11 |
± 0.13 |
± 0.14 |
± 0.070 |
± 0.080 |
± 0.090 |
> 1.60 |
≤ 2.00 |
± 0.14 |
± 0.15 |
± 0.16 |
± 0.080 |
± 0.090 |
± 0.110 |
> 2.00 |
≤ 2.50 |
± 0.16 |
± 0.17 |
± 0.18 |
± 0.110 |
± 0.120 |
± 0.130 |
> 2.50 |
≤ 3.00 |
± 0.19 |
± 0.20 |
± 0.20 |
± 0.130 |
± 0.140 |
± 0.150 |
> 3.00 |
≤ 5.00 |
± 0.22 |
± 0.24 |
± 0.25 |
± 0.17 |
± 0.18 |
± 0.19 |
> 5.00 |
≤ 6.50 |
± 0.24 |
± 0.25 |
± 0.26 |
± 0.19 |
± 0.20 |
± 0.21 |
1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm
The following tolerances apply to the steel grades with a minimum value for the yield strength 360N/mm² ≤ Rp0.2 ≤ 420N/mm².
Nominal |
Normal tolerances for a nominal width of 1 2 |
Special tolerances (S) for a |
|||||
---|---|---|---|---|---|---|---|
|
≤ 1200 |
> 1200 |
> 1500 |
≤ 1200 |
> 1200 |
> 1500 |
|
|
≤ 1500 |
|
|
≤ 1500 |
|
||
≥ 0.35 |
≤ 0.40 |
± 0.05 |
± 0.06 |
- |
± 0.040 |
± 0.045 |
- |
> 0.40 |
≤ 0.60 |
± 0.06 |
± 0.07 |
± 0.08 |
± 0.045 |
± 0.050 |
± 0.060 |
> 0.60 |
≤ 0.80 |
± 0.07 |
± 0.08 |
± 0.09 |
± 0.050 |
± 0.060 |
± 0.070 |
> 0.80 |
≤ 1.00 |
± 0.08 |
± 0.09 |
± 0.11 |
± 0.060 |
± 0.070 |
± 0.080 |
> 1.00 |
≤ 1.20 |
± 0.10 |
± 0.11 |
± 0.12 |
± 0.070 |
± 0.080 |
± 0.090 |
> 1.20 |
≤ 1.60 |
± 0.13 |
± 0.14 |
± 0.16 |
± 0.080 |
± 0.090 |
± 0.110 |
> 1.60 |
≤ 2.00 |
± 0.16 |
± 0.17 |
± 0.19 |
± 0.090 |
± 0.110 |
± 0.120 |
> 2.00 |
≤ 2.50 |
± 0.18 |
± 0.20 |
± 0.21 |
± 0.120 |
± 0.130 |
± 0.140 |
> 2.50 |
≤ 3.00 |
± 0.22 |
± 0.22 |
± 0.23 |
± 0.140 |
± 0.150 |
± 0.160 |
> 3.00 |
≤ 5.00 |
± 0.22 |
± 0.24 |
± 0.25 |
± 0.17 |
± 0.18 |
± 0.19 |
> 5.00 |
≤ 6.50 |
± 0.24 |
± 0.25 |
± 0.26 |
± 0.19 |
± 0.20 |
± 0.21 |
1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm.
The following tolerances apply to the steel grades with a minimum value for the yield strength 420N/mm² < Rp0.2 ≤ 900N/mm².
Nominal |
Normal tolerances for a nominal width of 1 2 |
Special tolerances (S) for a |
|||||
---|---|---|---|---|---|---|---|
|
≤ 1200 |
> 1200 |
> 1500 |
≤ 1200 |
> 1200 |
> 1500 |
|
|
≤ 1500 |
|
|
≤ 1500 |
|
||
≥ 0.35 |
≤ 0.40 |
± 0.06 |
± 0.07 |
- |
± 0.045 |
± 0.050 |
- |
> 0.40 |
≤ 0.60 |
± 0.06 |
± 0.08 |
± 0.09 |
± 0.050 |
± 0.060 |
± 0.070 |
> 0.60 |
≤ 0.80 |
± 0.07 |
± 0.09 |
± 0.11 |
± 0.060 |
± 0.070 |
± 0.080 |
> 0.80 |
≤ 1.00 |
± 0.09 |
± 0.11 |
± 0.12 |
± 0.070 |
± 0.080 |
± 0.090 |
> 1.00 |
≤ 1.20 |
± 0.11 |
± 0.13 |
± 0.14 |
± 0.080 |
± 0.090 |
± 0.110 |
> 1.20 |
≤ 1.60 |
± 0.15 |
± 0.16 |
± 0.18 |
± 0.090 |
± 0.110 |
± 0.120 |
> 1.60 |
≤ 2.00 |
± 0.18 |
± 0.19 |
± 0.21 |
± 0.110 |
± 0.120 |
± 0.140 |
> 2.00 |
≤ 2.50 |
± 0.21 |
± 0.22 |
± 0.24 |
± 0.140 |
± 0.150 |
± 0.170 |
> 2.50 |
≤ 3.00 |
± 0.24 |
± 0.25 |
± 0.26 |
± 0.170 |
± 0.180 |
± 0.190 |
> 3.00 |
≤ 5.00 |
± 0.26 |
± 0.27 |
± 0.28 |
± 0.23 |
± 0.24 |
± 0.26 |
> 5.00 |
≤ 6.50 |
± 0.28 |
± 0.29 |
± 0.30 |
± 0.25 |
± 0.26 |
± 0.28 |
1. Around cold-rolled welds an increase of 20% at the most over the thickness tolerance is allowed
over a length of 15 metres.
2. For zinc coatings ≥ Z450 the tolerance on the thickness must be raised by 0.02mm.
Tolerances on width
The tolerances on width comply with standard EN 10143: 2006
MagiZinc is not included in the standard, but fulfils EN 10143: 2006 requirements.
Tighter tolerances are available on request.
Tolerances in mm.
Nominal width w | Normal tolerances | Special tolerances (S) |
---|---|---|
600 ≤ w ≤ 1200 | + 5 0 |
+ 2 0 |
1200 < w ≤ 1500 | + 6 0 |
+ 2 0 |
1500 < w ≤ 1800 | + 7 0 |
+ 3 0 |
w > 1800 | + 8 0 |
+ 3 0 |
Dimensions and coil weights
Description | Availability |
---|---|
Coil diameter inner | 610mm |
(508 mm available on request) | |
Coil diameter outer | 10/7 x width max |
1000mm min. | |
2500mm max. | |
Coil weight | 30t max. |
33t max available after consultation | |
Coil weight limited by maximum outer diameter | |
Maximum weight allowed by road/rail transport | |
Some products may have different coil weight ranges available | |
Usually a minimum coil weight up to 85% of the maximum coil weight can be requested | |
KIM: width ≤ 1200 mm | 11.7 - 22.7 kg/mm width |
KIM: 1200mm < width ≤ 1700 mm | 11.6 - 21.7 kg/mm width |
KIM: width > 1700 mm | 11.0 kg/mm width and 11.6 - 21.7 kg/mm width |
Minimum tonnage per order | Refer to price list for order quantity details |
Minimum order quantities may apply |
EN-EngineeringAutomotive-Product-Metallic coated-All grades Further processing
Further processing
We have a broad network of Tata Steel service centres across Europe, offering decoiling and slitting services from stock and against short lead times
Light gauge processing
Processing type | Slitting | Decoiling | Blanking |
---|---|---|---|
Thickness range (mm) | 0.2 - 7.0 | 0.3 - 6.0 | 0.3 - 6.0 |
Width range (mm) | 10 - 2050 | 50 - 2600 | 200 - 2600 |
Length range | - | up to 6m | up to 6m |
Locations | UK Ireland Netherlands Germany France Spain Sweden Norway Finland |
UK Ireland Netherlands Germany France Spain Sweden Norway Finland |
UK Netherlands |
For further information please visit our Service Centre webpages.